2022 High quality Aluminum Mig Welding Wire - JQ.MH00Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao


Product Detail

Product Tags

Related Video

Feedback (2)

Our target should be to consolidate and enhance the top quality and service of current goods, in the meantime frequently create new products to satisfy diverse customers' calls for for 2 X 2 Wire Mesh, Flux Core Stainless Steel, 309 Flux Core Wire, Being a young increasing organization, we might not the best, but we have been trying our best for being your very good partner.
2022 High quality Aluminum Mig Welding Wire - JQ.MH00Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao Detail:

Features

Compared with manual welding, the deposition speed can be increased by 2-4 times, and the deposition efficiency is as high as 90%.

The adaptability of current and voltage is large, the setting of welding conditions is easy, and it is easy to carry out semi-automatic and automatic welding.

Good slag removal and glossy weld bead surface. In addition, there is little splash, the arc stability is excellent, and the X-ray is qualified.

Welding wire chemical composition(Wt%)

Model

Welding wire chemical composition(Wt%)

C

Mn

Si

Cr

Ni

P

S

Cu

other

JQ.MH00Cr24Ni13

0.026

1.74

0.58

23.49

12.9

0.024

0.008

-

-

Product performance

Compliant (equivalent) standard model

An example of physical properties of deposited metal (with SJ601)

GB

AWS

Tensile StrengthMPa

Elongation%

F309L-H00Cr24Ni13

ER309L

558

40.0

Product welding reference current(AC or DC+)

Diameter(mm)

¢2.5

¢3.2

¢4.0

¢5.0

Welding current(A)

400-500

450-550

500-600

550-650

Product Specifications

Wire diameter

¢2.5

¢3.2

¢4.0

¢5.0

Package weight

25/50/100/200/250/300/350Kg/piece

Precautions for product use

1. The temperature between welds is recommended to be controlled at about 150°C. When multi-pass multi-layer welding of small and medium-sized specifications, pay attention to controlling the welding line energy.
2. The rust layer, moisture, oil, dust, etc. of the welding part must be cleaned up.
3. The flux must be baked at 300-350℃ for 2h before use.
The above suggestions are for reference only, and the actual situation shall prevail in the specific operation. If necessary, process qualification should be carried out before determining the welding plan.


Product detail pictures:

2022 High quality Aluminum Mig Welding Wire - JQ.MH00Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao detail pictures


Related Product Guide:

We know that we only thrive if we can guarantee our combined price tag competiveness and top quality advantageous at the same time for 2022 High quality Aluminum Mig Welding Wire - JQ.MH00Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao , The product will supply to all over the world, such as: Turkey, Jakarta, Korea, We welcome you to visit our company, factory and our showroom displayed various products that will meet your expectation, meanwhile, it is convenient to visit our website, our sales staff will try their efforts to offer you the best service. If you need to have more information, remember to do not hesitate to contact us by E-mail or telephone.
  • We feel easy to cooperate with this company, the supplier is very responsible, thanks.There will be more in-depth cooperation.
    5 Stars By Natalie from panama - 2017.03.28 12:22
    The factory technical staff gave us a lot of good advice in the cooperation process, this is very good, we are very grateful.
    5 Stars By Honorio from Somalia - 2018.09.29 13:24
    Write your message here and send it to us