We're going to dedicate ourselves to offering our esteemed shoppers with the most enthusiastically considerate solutions for Arc Welding Wire, Er 347h Filler Wire, 0.9 Mm Flux Cored Welding Wire, We warmly welcome domestic and overseas customers send inquiry to us ,we have 24hours working team! Anytime anywhere we are still here to be your partner.
China Manufacturer for Copper Alloy Welding Wire - JQ.MH00Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao Detail:

Features

Compared with manual welding, the deposition speed can be increased by 2-4 times, and the deposition efficiency is as high as 90%.

The adaptability of current and voltage is large, the setting of welding conditions is easy, and it is easy to carry out semi-automatic and automatic welding.

Good slag removal and glossy weld bead surface. In addition, there is little splash, the arc stability is excellent, and the X-ray is qualified.

Welding wire chemical composition(Wt%)

Model

Welding wire chemical composition(Wt%)

C

Mn

Si

Cr

Ni

P

S

Cu

other

JQ.MH00Cr24Ni13

0.026

1.74

0.58

23.49

12.9

0.024

0.008

-

-

Product performance

Compliant (equivalent) standard model

An example of physical properties of deposited metal (with SJ601)

GB

AWS

Tensile StrengthMPa

Elongation%

F309L-H00Cr24Ni13

ER309L

558

40.0

Product welding reference current(AC or DC+)

Diameter(mm)

¢2.5

¢3.2

¢4.0

¢5.0

Welding current(A)

400-500

450-550

500-600

550-650

Product Specifications

Wire diameter

¢2.5

¢3.2

¢4.0

¢5.0

Package weight

25/50/100/200/250/300/350Kg/piece

Precautions for product use

1. The temperature between welds is recommended to be controlled at about 150°C. When multi-pass multi-layer welding of small and medium-sized specifications, pay attention to controlling the welding line energy.
2. The rust layer, moisture, oil, dust, etc. of the welding part must be cleaned up.
3. The flux must be baked at 300-350℃ for 2h before use.
The above suggestions are for reference only, and the actual situation shall prevail in the specific operation. If necessary, process qualification should be carried out before determining the welding plan.


Product detail pictures:

China Manufacturer for Copper Alloy Welding Wire - JQ.MH00Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao detail pictures


Related Product Guide:

Our goods are broadly recognized and reliable by users and can meet consistently switching financial and social demands of China Manufacturer for Copper Alloy Welding Wire - JQ.MH00Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao , The product will supply to all over the world, such as: Kenya, UK, moldova, Due to our good products and services, we have received good reputation and credibility from local and international customers. If you need more information and are interested in any of our products, please feel free to contact us. We look forward to becoming your supplier in the near future.
  • This supplier stick to the principle of "Quality first, Honesty as base", it is absolutely to be trust.
    5 Stars By Penny from Qatar - 2018.06.18 17:25
    The sales manager is very patient, we communicated about three days before we decided to cooperate, finally, we are very satisfied with this cooperation!
    5 Stars By Ricardo from Colombia - 2018.09.12 17:18
    Write your message here and send it to us