Competitive Price for Sf1a Welding Wire - JQ.MH00Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao


Product Detail

Product Tags

Related Video

Feedback (2)

We persistently execute our spirit of ''Innovation bringing growth, Highly-quality making sure subsistence, Administration marketing reward, Credit history attracting clients for Royal Welding Wires Private Limited, Spot Welding Electrode Material, 0.8 Welding Wire, We give priority to quality and customer pleasure and for this we follow stringent excellent control measures. We've got in-house testing facilities where our items are tested on every single aspect at different processing stages. Owning to latest technologies, we facilitate our clients with custom made creation facility.
Competitive Price for Sf1a Welding Wire - JQ.MH00Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao Detail:

Features

Compared with manual welding, the deposition speed can be increased by 2-4 times, and the deposition efficiency is as high as 90%.

The adaptability of current and voltage is large, the setting of welding conditions is easy, and it is easy to carry out semi-automatic and automatic welding.

Good slag removal and glossy weld bead surface. In addition, there is little splash, the arc stability is excellent, and the X-ray is qualified.

Welding wire chemical composition(Wt%)

Model

Welding wire chemical composition(Wt%)

C

Mn

Si

Cr

Ni

P

S

Cu

other

JQ.MH00Cr24Ni13

0.026

1.74

0.58

23.49

12.9

0.024

0.008

-

-

Product performance

Compliant (equivalent) standard model

An example of physical properties of deposited metal (with SJ601)

GB

AWS

Tensile StrengthMPa

Elongation%

F309L-H00Cr24Ni13

ER309L

558

40.0

Product welding reference current(AC or DC+)

Diameter(mm)

¢2.5

¢3.2

¢4.0

¢5.0

Welding current(A)

400-500

450-550

500-600

550-650

Product Specifications

Wire diameter

¢2.5

¢3.2

¢4.0

¢5.0

Package weight

25/50/100/200/250/300/350Kg/piece

Precautions for product use

1. The temperature between welds is recommended to be controlled at about 150°C. When multi-pass multi-layer welding of small and medium-sized specifications, pay attention to controlling the welding line energy.
2. The rust layer, moisture, oil, dust, etc. of the welding part must be cleaned up.
3. The flux must be baked at 300-350℃ for 2h before use.
The above suggestions are for reference only, and the actual situation shall prevail in the specific operation. If necessary, process qualification should be carried out before determining the welding plan.


Product detail pictures:

Competitive Price for Sf1a Welding Wire - JQ.MH00Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao detail pictures


Related Product Guide:

Responsible excellent and fantastic credit rating standing are our principles, which will help us at a top-ranking position. Adhering towards the tenet of "quality initial, buyer supreme" for Competitive Price for Sf1a Welding Wire - JQ.MH00Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao , The product will supply to all over the world, such as: Swiss, Tajikistan, Bahrain, we are fully determined to control the whole supply chain so as to provide quality products at competitive price in a timely manner. We are keeping up with the advanced techniques, growing through creating more values for our clients and society.
  • This company conforms to the market requirement and joins in the market competition by its high quality product, this is an enterprise that have Chinese spirit.
    5 Stars By Joseph from Toronto - 2018.11.11 19:52
    Good quality and fast delivery, it's very nice. Some products have a little bit problem, but the supplier replaced timely, overall, we are satisfied.
    5 Stars By Steven from Jeddah - 2018.09.08 17:09
    Write your message here and send it to us