We also supply merchandise sourcing and flight consolidation companies. We now have our very own manufacturing facility and sourcing business. We could present you with almost every kind of product relevant to our solution array for Welding Wires Together, 307 Stainless Steel Welding Wire, Aluminum Mig Welding, "Making the Products of Large Quality" is definitely the everlasting purpose of our enterprise. We make unremitting endeavours to know the target of "We Will Always Hold in Pace along with the Time".
factory low price Flux Core Welding Wire - JQ.MH1Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao Detail:

Application

It is often used in the welding of carbon steel and stainless steel dissimilar materials or in the welding of martensitic and pearlitic stainless steels with poor toughness. Applications such as petrochemical, thermal power plants and other industries.

Welding wire chemical composition(Wt%)

Model

Welding wire chemical composition(Wt%)

C

Mn

Si

Cr

Ni

P

S

Cu

other

JQ.MH1Cr24Ni13

0.051

1.79

0.56

23.84

13.10

0.024

0.012

0.13

Mo:0.20

Product performance

Compliant (equivalent) standard model

An example of physical properties of deposited metal (with SJ601)

GB

AWS

Tensile StrengthMPa

Elongation%

F309-H1Cr24Ni13

ER309

599

36.0

Product welding reference current(AC or DC+)

Diameter(mm)

¢2.5

¢3.2

¢4.0

¢5.0

Welding current(A)

400-500

450-550

500-600

550-650

Product Specifications

Wire diameter

¢2.5

¢3.2

¢4.0

¢5.0

Package weight

25/50/100/200/250/300/350Kg/piece

Precautions for product use

1. The temperature between welds is recommended to be controlled at about 150°C. When multi-pass multi-layer welding of small and medium-sized specifications, pay attention to controlling the welding line energy.
2. The rust layer, moisture, oil, dust, etc. of the welding part must be cleaned up.
3. The flux must be baked at 300-350℃ for 2h before use.
The above suggestions are for reference only, and the actual situation shall prevail in the specific operation. If necessary, process qualification should be carried out before determining the welding plan.


Product detail pictures:

factory low price Flux Core Welding Wire - JQ.MH1Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao detail pictures


Related Product Guide:

We hold strengthening and perfecting our items and repair. At the same time, we get the job done actively to do research and progress for factory low price Flux Core Welding Wire - JQ.MH1Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao , The product will supply to all over the world, such as: Madras, Auckland, Adelaide, By adhering to the principle of "human oriented, winning by quality", our company sincerely welcomes merchants from at home and abroad to visit us, talk business with us and jointly create a brilliant future.
  • A nice supplier in this industry, after a detail and careful discussion, we reached a consensus agreement. Hope that we cooperate smoothly.
    5 Stars By Modesty from Belgium - 2017.09.29 11:19
    The company has a good reputation in this industry, and finally it tured out that choose them is a good choice.
    5 Stars By Miriam from Lahore - 2017.08.21 14:13
    Write your message here and send it to us