To get the stage of realizing dreams of our employees! To build a happier, more united and much more skilled crew! To reach a mutual benefit of our prospects, suppliers, the society and ourselves for Gasless Mig Welding Wire, Copper Welding Wire, Flux Core Welding Stainless Steel, We sincerely look forward to hearing from you. Give us a chance to show you our professionalism and passion. We are sincerely welcome good friends from numerous circles at dwelling and abroad come to cooperate!
Hot New Products Submerged-Arc Welding Wire - JQ.MH00Cr21Ni10T stainless steel submerged-arc welding wire – Jinqiao Detail:

Application

Mainly for CNG (compressed natural gas), LNG (liquefied natural gas), LPG (liquefied petroleum gas) energy equipment field for welding stainless steel materials used in cryogenic and low temperature environments; such as 12Cr18Ni9 (SUS 302), 06Cr19Ni10 (SUS 304), 022Cr18Ni9 (SUS 304L) ) welding.

Welding wire chemical composition(Wt%)

Model

Welding wire chemical composition(Wt%)

C

Mn

Si

Cr

Ni

P

S

Cu

other

JQ.MH00Cr21Ni10T

0.027

1.75

0.57

20.27

9.56

0.023

0.010

-

-

Product performance

Compliant (equivalent) standard model

An example of physical properties of deposited metal (with SJ601)

GB

AWS

Tensile StrengthMPa

Elongation%

F308L-H00Cr21Ni10

ER308L

568

35.5

Product welding reference current(AC or DC+)

Diameter(mm)

¢2.5

¢3.2

¢4.0

¢5.0

Welding current(A)

400-500

450-550

500-600

550-650

Product Specifications

Wire diameter

¢2.5

¢3.2

¢4.0

¢5.0

Package weight

25/50/100/200/250/300/350Kg/piece

Precautions for product use

1. The temperature between welds is recommended to be controlled at about 150°C. When multi-pass multi-layer welding of small and medium-sized specifications, pay attention to controlling the welding line energy.
2. The rust layer, moisture, oil, dust, etc. of the welding part must be cleaned up.
3. The flux must be baked at 300-350℃ for 2h before use.
The above suggestions are for reference only, and the actual situation shall prevail in the specific operation. If necessary, process qualification should be carried out before determining the welding plan.


Product detail pictures:

Hot New Products Submerged-Arc Welding Wire - JQ.MH00Cr21Ni10T stainless steel submerged-arc welding wire – Jinqiao detail pictures


Related Product Guide:

Our company insists all along the quality policy of "product quality is base of enterprise survival; customer satisfaction is the staring point and ending of an enterprise; persistent improvement is eternal pursuit of staff" and the consistent purpose of "reputation first, customer first" for Hot New Products Submerged-Arc Welding Wire - JQ.MH00Cr21Ni10T stainless steel submerged-arc welding wire – Jinqiao , The product will supply to all over the world, such as: Angola, Roman, Mali, We always insist on the principle of "Quality and service are the life of the product". Till now, our products have been exported to more than 20 countries under our strict quality control and high level service.
  • The enterprise has a strong capital and competitive power, product is sufficient, reliable, so we have no worries on cooperating with them.
    5 Stars By Matthew Tobias from Juventus - 2017.09.30 16:36
    A good manufacturers, we have cooperated twice, good quality and good service attitude.
    5 Stars By Maggie from Palestine - 2017.08.16 13:39
    Write your message here and send it to us