We insist on offering high-quality creation with superior business enterprise concept, honest revenue plus the greatest and fast service. it will bring you not only the high quality solution and huge profit, but essentially the most significant is usually to occupy the endless market for Wire Butt Welding Machine, Dual Shield Stainless Wire, Magnesium Welding Wire, You would not have any communication problem with us. We sincerely welcome prospects all around the globe to call us for business enterprise cooperation.
Manufactur standard Cast Iron Mig Welding Wire - JQ.MH00Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao Detail:

Features

Compared with manual welding, the deposition speed can be increased by 2-4 times, and the deposition efficiency is as high as 90%.

The adaptability of current and voltage is large, the setting of welding conditions is easy, and it is easy to carry out semi-automatic and automatic welding.

Good slag removal and glossy weld bead surface. In addition, there is little splash, the arc stability is excellent, and the X-ray is qualified.

Welding wire chemical composition(Wt%)

Model

Welding wire chemical composition(Wt%)

C

Mn

Si

Cr

Ni

P

S

Cu

other

JQ.MH00Cr24Ni13

0.026

1.74

0.58

23.49

12.9

0.024

0.008

-

-

Product performance

Compliant (equivalent) standard model

An example of physical properties of deposited metal (with SJ601)

GB

AWS

Tensile StrengthMPa

Elongation%

F309L-H00Cr24Ni13

ER309L

558

40.0

Product welding reference current(AC or DC+)

Diameter(mm)

¢2.5

¢3.2

¢4.0

¢5.0

Welding current(A)

400-500

450-550

500-600

550-650

Product Specifications

Wire diameter

¢2.5

¢3.2

¢4.0

¢5.0

Package weight

25/50/100/200/250/300/350Kg/piece

Precautions for product use

1. The temperature between welds is recommended to be controlled at about 150°C. When multi-pass multi-layer welding of small and medium-sized specifications, pay attention to controlling the welding line energy.
2. The rust layer, moisture, oil, dust, etc. of the welding part must be cleaned up.
3. The flux must be baked at 300-350℃ for 2h before use.
The above suggestions are for reference only, and the actual situation shall prevail in the specific operation. If necessary, process qualification should be carried out before determining the welding plan.


Product detail pictures:

Manufactur standard Cast Iron Mig Welding Wire - JQ.MH00Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao detail pictures


Related Product Guide:

The customer satisfaction is our primary target. We uphold a consistent level of professionalism, quality, credibility and service for Manufactur standard Cast Iron Mig Welding Wire - JQ.MH00Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao , The product will supply to all over the world, such as: Birmingham, Czech, United Arab Emirates, We have 48 provincial agencies in the country. We also have stable cooperation with several international trading companies. They place order with us and export products to other countries. We expect to cooperate with you to develop a larger market.
  • On this website, product categories is clear and rich, I can find the product I want very quickly and easily, this is really very good!
    5 Stars By Andy from Italy - 2017.04.18 16:45
    We always believe that the details decides the company's product quality, in this respect, the company conform our requirements and the goods are meet our expectations.
    5 Stars By Monica from Cannes - 2017.11.12 12:31
    Write your message here and send it to us