Wholesale Price Silicon Bronze Welding Wire - JQ.MH1Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao


Product Detail

Product Tags

Related Video

Feedback (2)

Our enterprise since its inception, often regards solution excellent as enterprise life, continually strengthen output technology, enhance product high quality and continually strengthen organization total high-quality administration, in strict accordance using the national standard ISO 9001:2000 for Mig Welding Stainless Steel, Dual Shield Welding, Stainless Steel Welding Wire For Mig, We warmly welcome domestic and overseas customers send inquiry to us ,we have 24hours working team! Anytime anywhere we are still here to be your partner.
Wholesale Price Silicon Bronze Welding Wire - JQ.MH1Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao Detail:

Application

It is often used in the welding of carbon steel and stainless steel dissimilar materials or in the welding of martensitic and pearlitic stainless steels with poor toughness. Applications such as petrochemical, thermal power plants and other industries.

Welding wire chemical composition(Wt%)

Model

Welding wire chemical composition(Wt%)

C

Mn

Si

Cr

Ni

P

S

Cu

other

JQ.MH1Cr24Ni13

0.051

1.79

0.56

23.84

13.10

0.024

0.012

0.13

Mo:0.20

Product performance

Compliant (equivalent) standard model

An example of physical properties of deposited metal (with SJ601)

GB

AWS

Tensile StrengthMPa

Elongation%

F309-H1Cr24Ni13

ER309

599

36.0

Product welding reference current(AC or DC+)

Diameter(mm)

¢2.5

¢3.2

¢4.0

¢5.0

Welding current(A)

400-500

450-550

500-600

550-650

Product Specifications

Wire diameter

¢2.5

¢3.2

¢4.0

¢5.0

Package weight

25/50/100/200/250/300/350Kg/piece

Precautions for product use

1. The temperature between welds is recommended to be controlled at about 150°C. When multi-pass multi-layer welding of small and medium-sized specifications, pay attention to controlling the welding line energy.
2. The rust layer, moisture, oil, dust, etc. of the welding part must be cleaned up.
3. The flux must be baked at 300-350℃ for 2h before use.
The above suggestions are for reference only, and the actual situation shall prevail in the specific operation. If necessary, process qualification should be carried out before determining the welding plan.


Product detail pictures:

Wholesale Price Silicon Bronze Welding Wire - JQ.MH1Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao detail pictures


Related Product Guide:

Bear "Customer 1st, Good quality first" in mind, we work closely with our prospects and supply them with efficient and professional services for Wholesale Price Silicon Bronze Welding Wire - JQ.MH1Cr24Ni13 stainless steel submerged-arc welding wire – Jinqiao , The product will supply to all over the world, such as: Israel, Zurich, Albania, We warmly welcome domestic and overseas customers to visit our company and have business talk. Our company always insists on the principle of "good quality, reasonable price, the first-class service". We are willing to build long-term, friendly and mutually beneficial cooperation with you.
  • After the signing of the contract, we received satisfactory goods in a short term, this is a commendable manufacturer.
    5 Stars By Linda from Macedonia - 2017.04.18 16:45
    The sales manager has a good English level and skilled professional knowledge, we have a good communication. He is a warm and cheerful man, we have a pleasant cooperation and we became very good friends in private.
    5 Stars By Nainesh Mehta from Mauritius - 2017.12.19 11:10
    Write your message here and send it to us